Kiribati 347 Stainless Steel Bar
Category:
Product Description
347 Stainless Steel Bar Description
347 stainless steel is more durable than other stainless steel materials under high temperatures. This makes it very popular for use in high temperature environments. 347 stainless steel maintains its strength and durability without embrittlement or fatigue in high-temperature yet corrosive environments. Its ability to remain stable in corrosive environments with strong acids and bases such as chloride ions and sulfide ions makes it ideal for use in the chemical and petroleum industries. In addition, 347 stainless steel also has good processing properties. That is why the bars can be processed into various shapes by various methods such as forging, quenching, annealing and cold working. They are commonly seen as manufacturing parts in industries such as chemical, petroleum, pharmaceutical and food processing due to high temperature durability, corrosion resistance and processability.
Product Parameters
|
Product Name |
347 Stainless Steel Bar |
|
|
Type |
Steel Bar |
|
|
Outer Diameter |
Round Bar |
4mm-500mm |
|
Hexagon Bar |
18mm-57mm (11/16″ to 2-3/4″) |
|
|
Square Bar |
18mm-47mm (11/16″ to 1-3/4″) |
|
|
Flat Steel |
1/2 "to 10", Thickness: 2mm-150mm, Can provide customized |
|
|
Length |
1-6 meters, Length can be customized |
|
|
Standard |
ASTM, AISI, JIS, GB, DIN, EN, etc. |
|
|
Surface |
Black, Bright Polished, Rough Turning, Mattness Surface Treatment, No. 4. BA, etc. |
|
|
Scope of Application |
Stainless steel bars are used in a variety of industries such as shipbuilding, Defense, Automotive, Textiles, Paper and pulp, Manufacturing, Cement, Heavy earthmoving equipment and construction, etc. |
|
Chemical Composition
|
C |
Si |
Mn |
Cr |
Ni |
S |
P |
|
≤ 0.08 |
≤ 0.75 |
≤ 2.0 |
18.0~20.0 |
9.0~13.0 |
≤ 0.03 |
≤ 0.04 |
Mechanical Properties
|
Tensile Strength Kb (MPa) |
Yield Strength σ0.2 (MPa) |
Elongation D5 (%) |
Hardness |
|
≥515 |
≥205 |
≥ 40 |
≤ 201HB;≤ 95HRB |
Physical Performance
|
Density(g/cm³) |
Modulus of Elasticity(Gpa) |
Coefficient of Thermal Expansion(10-6/°C) |
Coefficient of Thermal Conductivity(W/m*K) |
Resistivity(ΜΩ. cm) |
|
7.97 |
193 |
16.0 |
16.3 |
72 |